A form of steel pipe known as stainless steel welded pipes is created by joining two or more pieces of stainless steel together. The method of welding utilised might vary, but common methods include plasma welding, MIG (metal inert gas) welding, and TIG (tungsten inert gas) welding.
Numerous industries, including those in the petrochemical, chemical, food processing, and water treatment sectors, use stainless steel welded pipes. They are also employed for structural and architectural purposes. Welded pipes are frequently more affordable and simpler to produce than seamless pipes, making them a preferred option in many sectors.
Standard: | ASTM, ASME, DIN, BS, EN, IS, AMS, JIS, IBR & Other International Standards. |
Dimensions: | ASTM A 312 ASME SA 312 / ASTM A 358 ASME SA 358 |
Size: | 1/8NB TO 30NB IN |
SS Pipes: | 1/2" NB - 16" NB |
ERW Pipes: | 1/2" NB - 24" NB |
EFW Pipes: | 6" NB - 100" NB |
Specialized in: | Large Diameter Size |
Schedule: | SCH 5, SCH10, SCH 20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
Type: | Seamless / ERW / Welded / Fabricated / CDW |
Form: | Round Pipes, Square Pipes, Rectangular Pipes, etc. |
Length : | Single Random, Double Random & Required Length |
End : | Plain End, Beveled End, Treaded |
SEND US YOUR REQUIREMENT NOW
Element | Typical Range |
---|---|
Carbon (C) | 0-0.03% |
Manganese (Mn) | 0-2.00% |
Phosphorus (P) | 0-0.045% |
Sulfur (S) | 0-0.03% |
Silicon (Si) | 0-1.00% |
Chromium (Cr) | 10.5-30.00% |
Nickel (Ni) | 8.0-25.00% |
Molybdenum (Mo) | 0-7.00% |
Titanium (Ti) | 0-0.70% |
Property | Value |
---|---|
Density | 7.9 to 8.05 g/cm3 |
Melting point | 1370 to 1425°C |
Thermal conductivity | 15 W/mK |
Electrical conductivity | 3.5% IACS |
Magnetic properties | Austenitic grades (e.g. 304, 316) are generally non-magnetic, while ferritic and martensitic grades can be magnetic |
Yield strength | 170 to 550 MPa |
Grade | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
---|---|---|---|---|---|
304/ 304L | 8.0 g/cm3 | 1400 °C (2550 °F) | Psi 75000 , MPa 515 | Psi 30000 , MPa 205 | 35 % |
304H | 8.0 g/cm3 | 1400 °C (2550 °F) | Psi 75000 , MPa 515 | Psi 30000 , MPa 205 | 40 % |
310 / 310S / 310H | 7.9 g/cm3 | 1402 °C (2555 °F) | Psi 75000 , MPa 515 | Psi 30000 , MPa 205 | 40 % |
306/ 316H | 8.0 g/cm3 | 1400 °C (2550 °F) | Psi 75000 , MPa 515 | Psi 30000 , MPa 205 | 35 % |
316L | 8.0 g/cm3 | 1399 °C (2550 °F) | Psi 75000 , MPa 515 | Psi 30000 , MPa 205 | 35 % |
317 | 7.9 g/cm3 | 1400 °C (2550 °F) | Psi 75000 , MPa 515 | Psi 30000 , MPa 205 | 35 % |
321 | 8.0 g/cm3 | 1457 °C (2650 °F) | Psi 75000 , MPa 515 | Psi 30000 , MPa 205 | 35 % |
347 | 8.0 g/cm3 | 1454 °C (2650 °F) | Psi 75000 , MPa 515 | Psi 30000 , MPa 205 | 35 % |
904L | 7.95 g/cm3 | 1350 °C (2460 °F) | Psi 71000 , MPa 490 | Psi 32000 , MPa 220 | 35 % |